dc.description.abstractTurkish feldspars containing some amounts of mineral phases bearing iron and titanium impurities have been studied by the flotation benefication method. On the benefication experiments with the potassium feldspar, the best condition were obtained by using a sulphonate type collector-R840 with 3 stage flotation. Fe2O3 content was decreased from 0.49% to 0.23% and TiO2 content was increased from 0.06% to 0.04%. K2O content was increased from 8.66% up to 9.82% and Na2O content from 2.32% to 2.73%. On the benefication experiments with the sodium feldspar, the best condition was obtained by using sodium oleate collector with 3-stage flotation. TiO2 content was decreased from 0.55% to 0.23% and Fe2O3 content from 0.17% to 0.13%. Na2O content decreased from 10.39% to 8.80% and K2O content from 0.90 to 0.63%.en_US
dc.language.isoengen_US
dc.publisherTechna Srlen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.titleBenefication of Turkish feldspars by flotation methodsen_US
dc.typearticleen_US
dc.relation.journalIndustrial Ceramicsen_US
dc.contributor.departmentAnadolu Üniversitesien_US
dc.identifier.volume15en_US
dc.identifier.issue3en_US
dc.identifier.startpage158en_US
dc.identifier.endpage162en_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster