Ara
Toplam kayıt 6, listelenen: 1-6
Preparation of cordierite ceramics from talc with boron oxide addition
(2004)
Thermal reactions of impure materials of talc, silica and alumina with moderate particle sizes were investigated to obtain a dense cordierite ceramic by boron oxide addition as a sintering aid. Mixed powders were uniaxially ...
Thermal shock behaviour of alumina-mullite-zircon refractories
(Trans Tech Publications LTD, 2004)
Thermal shock behaviour of alumina-mullite-zircon refractories was investigated by varying zircon content. Thermal shock parameters R and R-st based on the room temperature mechanical measurements were calculated as a ...
The influence of fine alumina particles on the mechanical properties and thermal shock behaviour of slip-cast alumina-mullite refractories
(Trans Tech Publications LTD, 2004)
The object of this work is to improve understanding of relationships between microstructure and those mechanical properties likely to affect thermal shock behaviour of slip-cast alumina-mullite refractories. The incorporation ...
Lanthanum titanate (La2Ti2O7) as an interphase material in alumina (Al2O3) based composites
(Trans Tech Publications LTD, 2004)
The aim of this research is to fabricate and characterize alumina (Al2O3) / lanthanum titanate (La2Ti2O7) laminate ceramic composites. The interfacial bond between oxide laminates has a critical effect on the final mechanical ...
Mechanical properties of alumina-mullite-zircon refractories
(Trans Tech Publications LTD, 2004)
The relationships between mechanical properties and microstructure of alumina-mullite-zircon refractories were investigated by varying zircon content. Various sintering temperatures were used for the slip-cast refractories ...
The corrosion resistance of alumina-mullite-zircon refractories in molten glass
(Trans Tech Publications LTD, 2004)
Corrosion measurements on a set of alumina-mullite-zircon refractories have been carried out using a static crucible test consisting of a "hole in a block". Rates of corrosion of the refractory at 1370 degreesC for 72 h ...